Bumper and spoiler, deep scratches and cracks
Bumper and spoiler, deep scratches and cracks |
1. |
Clean the component. It is important to insure that there is no gravel or other particles in the welding area.
|
2. |
Clean the area to be repaired with Teroson FL cleaner.
|
3. |
Identify the type of plastic. See
Plastic codes, temperature and welding wire
or
Plastic code table
.
|
4. |
Select the correct welding wire and set the welding gun to an operating temperature appropriate for the plastic type. See
Plastic codes, temperature and welding wire
|
5. |
If the damage is a crack, first drill at the ends so the crack does not spread. Use a 3.5 mm bit to drill a hole at each end of the crack.
|
6. |
Cut a 90° V-joint on the back. Use a low-speed machine.
|
7. |
Set the welding gun to an operating temperature appropriate for the plastic type. See
|
8. |
Weld the crack on the back.
|
9. |
Grind away any paint around the damaged area on the front.
|
10. |
Check the operating temperature of the gun.
|
11. |
Weld the front using welding wire.
|
12. |
Allow the welded area to cool.
|
13. |
Grind away excess welding material from the welded area.
|
14. |
Carry out final steps 1 - 10. See
Bumper, scratches and scrapes
.
|