A-pillar outer panel, CV
| A-pillar outer panel, CV | 
Certain welded joints on the car may be MIG brazed with bronze as the filling material. A MIG brazed seam may be recognized from the gold colour of the joint. A MIG brazing must always be replaced by a new MIG brazing.
        
  | 
      |||||||
| 1. | 
        Position the car in an aligning bench and cross-measure if necessary.
         | 
      |
| 2. | 
        Remove the
        
         Front wing
        
        ,
        
         Bonnet
        
        and
        
         Door
        
        .
         | 
      |
| 3. | 
        Drill out the spot welds as illustrated. Drill out the upper welds only so that the nut piece follows.
         
        
         | 
      |
| 4. | 
        Grind away the welds, according to the illustration. Note that the seam welds are MIG brazed.
         | 
      |
| 5. | 
        Knock loose the reinforcement.
         | 
      |
| 6. | 
        Cut the windscreen frame outer panel 250 mm from the outer edge of the A-pillar. Do not cut the underlying panel.
         
        
         | 
      |
| 7. | 
        Grind the seam welds as illustrated.
         | 
      |
| 8. | 
        Drill out the spot welds holding the A-pillar outer panel.
         | 
      |
| 9. | 
        Tap away the A-pillar outer panel and align any deformed sheet metal or panels.
         | 
      |
| 10. | 
        Drill holes for plug welding in the new A-pillar outer panel.
        
  | 
      |||||||||||||
| 11. | 
        Apply welding primer to the surfaces to be plug welded. Use Teroson Zink Spray
         | 
      |
| 12. | 
        Place the A-pillar outer panel in fitting position and secure it with welding clamps.
         | 
      |
| 13. | 
        Align the A-pillar outer panel exactly.
         | 
      |
| 14. | 
        Plug weld the A-pillar outer panel.
        
  
        
         | 
      ||||||||||
| 15. | 
        All-weld the joint at the upper end of the upper A-pillar outer panel.
         | 
      |
| 16. | 
        Seam weld the A-pillar outer panel as illustrated.
         | 
      |
| 18. | 
        Seam weld and continuous weld on the outside of the front wheel housing. Note that the welds must be MIG brazed.
         | 
      |
| 19. | 
        Wash away surplus welding primer. Welding primer reduces the adhesion of paint, filler and sealant.
         | 
      |
| 20. | 
        Apply primer to all bare metal surfaces. Use Standox 1K.
         | 
      |
| 21. | 
        Use Terostat 1K-PUR to seal joints and metal folds.
         | 
      |
| 22. | 
        Apply anti-corrosion agent to internal surfaces after painting. Use Terotex HV 400.
         | 
      |
| 23. | 
        Fit the
        
         Front wing
        
        ,
        
         Bonnet
        
        and
        
         Door
        
        .
         | 
      |

                Warning